The four-step process at a glance
Step 1
Heat
Heat the sheet in ~70 °C water until pliable.
Step 2
Form
Mold the softened sheet to the limb.
Step 3
Cool
Hold in place as it hardens.
Step 4
Fit & Adjust
Secure, then reheat to refine the fit.